Wraptor Plus™ has been tested by independant, nationally accredited testing firms. The following standards were used to obtain test results:
ASTM E 1677, ASTM E 96, ASTM E 84, ASTM D 1117, ASTM D 882, TAPPI T-410, AATCC 127, TAPPI T-460
|
| PROPERTIES |
TEST METHOD |
RESULTS |
| Thickness |
|
.0004 in. (nominal) |
| Basis Weight |
TAPPI-410 |
97.8 g/m² |
| Temperature Resistance |
FED SPEC HHB-1008 |
(-)40°F to 220°F |
Surface Burning Characteristics |
ASTM E 84-03 |
15 FSI (Class A)
40 SDI (Class A) |
| Tear Resistance |
ASTM D 1117 |
67.1 lbs. MD
91.2 lbs. CD |
| Breaking Strength |
ASTM D 882 |
27.2 lbs. MD
69.8 lbs. CD |
| Air Permeability |
TAPPI T-460 |
191.6 cfm/ft² |
| Water Penetration Resistance |
AATCC 127 |
>116.8 cm of H2O |
| Water Vapor Transmission |
ASTM E 96 A |
7 perms |
| Emmissivity |
ASTM C 1371 |
.06 - .07 |
|